The strength of Al2O3/SiC nanocomposites after grinding and annealing

Abstract:

Alumina matrix nanocomposites containing about 5 vol.% SiC of < 100 nm mean particle size show a substantial increase in strength after machining and annealing. The final strength is controlled by the annealing process and achieves the same level after a coarse machining using 150-grit diamond as is achieved using a complex lapping and polishing sequence. In all cases the final anneal leads to an increase in strength. The nanocomposite retains a significantly higher residual surface-compre...

Expand abstract
Publication status:
Published

Actions


Access Document


Authors


Lawrence, CW More by this author
More by this author
Institution:
University of Oxford
Department:
Oxford, MPLS, Materials
Volume:
46
Issue:
11
Pages:
3839-3848
Publication date:
1998-07-01
DOI:
ISSN:
1359-6454
URN:
uuid:80b773f8-9a23-4d7c-99e7-a58ceeaea4a8
Source identifiers:
15000
Local pid:
pubs:15000

Terms of use


Metrics



If you are the owner of this record, you can report an update to it here: Report update to this record

TO TOP