Thesis
Microstructural characterization of a 4043 Al alloy produced by molten metal deposition (MMD)
- Abstract:
-
Additive manufacturing (AM) encompasses a range of layer-by-layer fabrication techniques that have transformed modern manufacturing by enabling the production of complex geometries, reducing material waste, and offering unprecedented design flexibility. These advantages have made AM particularly attractive for industries such as aerospace, automotive and biomedical engineering. However, despite its growing adoption, conventional AM approaches—particularly powder- and laser-based processes—face several limitations, including high equipment and material costs, energy-intensive operation, and challenges related to process stability, residual stresses and microstructural control. In this context, molten metal deposition (MMD) has emerged as a promising wire-fed AM variant in which liquid metal is directly deposited. By eliminating the need for powders and high-energy laser systems, MMD offers a potentially more cost-effective and energy-efficient route, particularly suited for lower-melting-point alloys such as Al-Si alloys. Nevertheless, the relationships between processing parameters, layer geometry and microstructure in MMD remain insufficiently understood.
In this study, five 4043 aluminium alloy samples were fabricated by MMD under varying printing speeds, nozzle temperatures and substrate temperatures. The structures were analysed macroscopically and microscopically using optical microscopy and SEM, and quantification of primary α-Al grains and Fe-rich intermetallic compounds (IMCs). Interlayer junction width was sensitive to build height and processing conditions, reflecting the roles of wetting, spreading and prior-layer remelting. In contrast, grain structure and IMC characteristics remained relatively uniform across the processing window. The α-Al grains showed limited columnar features, while local Si enrichment at junctions indicated partial remelting of eutectic regions, enhancing interlayer bonding. Secondary dendrite arm spacing suggested cooling rates of ~10–100 K s⁻¹, sufficient for microstructural refinement despite being lower than in laser-based AM. Fe-rich IMCs were finely dispersed in interdendritic regions, with median lengths below 4 µm and minimal variation between layers.
Actions
Access Document
- Files:
-
-
(Preview, Dissemination version, pdf, 9.3MB, Terms of use)
-
Authors
Contributors
+ Liotti, E
- Institution:
- University of Oxford
- Division:
- MPLS
- Department:
- Materials
- Role:
- Supervisor
- ORCID:
- 0000-0002-9267-5157
+ Grant, P
- Institution:
- University of Oxford
- Division:
- MPLS
- Department:
- Materials
- Role:
- Supervisor
- ORCID:
- 0000-0002-7942-7837
- DOI:
- Type of award:
- MSc by Research
- Awarding institution:
- University of Oxford
- Language:
-
English
- Keywords:
- Deposit date:
-
2026-09-07
- ARK identifier:
Terms of use
- Copyright holder:
- Mingji Dai
- Copyright date:
- 2026
If you are the owner of this record, you can report an update to it here: Report update to this record